Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Terblend® N NG-04 - (ABS+PA6)-GF20 - INEOS Styrolution

Material Data Center offers the following functions for Terblend® N NG-04:
unit conversion, PDF datasheet print, comparison with other plastics, flow length calculation, snap fit calculation, beam deflection calculation, cooling time calculation, parameters for material models, CAE Interfaces

Check here, which other Terblend N datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informação do produto
Terblend® N NG-04 is a glass fibre reinforced ABS/PA blend with excellent dimensional stability, low mould shrinkage and high heat resistance.
Características de processamento/físicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Índice de fluidez volumétrico, MVR 15 / * cm³/10min ISO 1133
Temperatura 240 / * °C -
Carga 10 / * kg -
Contração após a moldagem, paralelo 0.3 / * % ISO 294-4, 2577
Contração após a moldagem, perpendicular 0.4 / * % ISO 294-4, 2577
Densidade do fundido 1070 kg/m³ -
Condutividade térmica do fundido 0.177 W/(m K) -
Capacidade térmica específica do fundido 2180 J/(kg K) -
Temperatura de ejeção 95 °C -
Propriedades mecânicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Módulo de tração 5400 / 4300 MPa ISO 527
Tensão na ruptura 60 / 50 MPa ISO 527
Deformação na ruptura 3.2 / 3.5 % ISO 527
Resistência ao impacto Charpy , +23°C 30 / - kJ/m² ISO 179/1eU
Resistência ao impacto Charpy, -30°C 25 / - kJ/m² ISO 179/1eU
Res. impacto Charpy c/entalhe, +23°C 8 / - kJ/m² ISO 179/1eA
Res. impacto Charpy c/entalhe, -30°C 5 / - kJ/m² ISO 179/1eA
Propriedades térmicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Temperatura de deflexão térmica, 1.80 MPa 100 / * °C ISO 75-1/-2
Temperatura de deflexão térmica, 0.45 MPa 164 / * °C ISO 75-1/-2
Temperatura de amolecimento Vicat, B 114 / * °C ISO 306
Coef. de expansão térmica linear, paralelo 40 / * E-6/K ISO 11359-1/-2
Flamabilidade a 1.5mm esp. nom. HB / * class IEC 60695-11-10
Espessuras do tubo de teste 1.6 / * mm -
Flamabilidade a espessura h HB / * class IEC 60695-11-10
Espessuras do tubo de teste 3.2 / * mm -
Propriedades elétricasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Constante dielétrica, 100Hz 3.6 / - - IEC 62631-2-1
Constante dielétrica, 1MHz 2.9 / 3.6 - IEC 62631-2-1
Fator de dissipação dielétrica, 1MHz 130 / 500 E-4 IEC 62631-2-1
Resistividade volumétrica específica 1E13 / 1E11 Ohm*m IEC 62631-3-1
Resistividade superficial específica * / 1E14 Ohm IEC 62631-3-2
Índice comparativo de linha de fuga 600 / 550 - IEC 60112
Outras propriedadesSeco / CondUnidadeMétodo de ensaio
Absorção de umidade 0.9 / * % Sim. to ISO 62
Densidade 1200 / - kg/m³ ISO 1183
Diagrama
Viscosidade - taxa de cisalhamento , Terblend® N NG-04, (ABS+PA6)-GF20, INEOS Styrolution
Tensão de cisalhamento - taxa de cisalhamento , Terblend® N NG-04, (ABS+PA6)-GF20, INEOS Styrolution
Tensão - deformação , Terblend® N NG-04 (dry), (ABS+PA6)-GF20, INEOS Styrolution
Módulo secante - deformação , Terblend® N NG-04 (dry), (ABS+PA6)-GF20, INEOS Styrolution
Volume específico - temperatura (pvT) , Terblend® N NG-04, (ABS+PA6)-GF20, INEOS Styrolution
Módulo de tração - temperatura , Terblend® N NG-04 (dry), (ABS+PA6)-GF20, INEOS Styrolution
Características
Processamento
Moldagem por injeção
Forma de entrega
Granulos
Características especiais
Antiestático
Disponibilidade regional
Outras informações
Moldagem por injeção
PREPROCESSING
Pre/Post-processing, Pre-drying, Temperature: 80 °C
Pre/Post-processing, Pre-drying, Time: 2 - 4 h

PROCESSING
injection molding, Melt temperature, range: 240 - 270 °C
injection molding, Melt temperature, recommended: 260 °C
injection molding, Mold temperature, range: 40 - 80 °C
injection molding, Mold temperature, recommended: 60 °C
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com